Add to Cart
Heat Resistant Zircon Mullite Brick Refractory High Temp Bricks ZM-20 ZM-11
Quick Detail:
1, High strength
2, Good thermal shock resistance
3, High temperature erosion resistance 
4, Good slag resistance
Description:
 
Zircon mullite brick selected high quality mullite sand and zircon powder as its main raw material. Molded by high pressure and sintered by high temperature , the zircon-mullite brick has such advantages as high bulk density, high strength, good thermal shock resistance, high temperature erosion resistance and good slag resistance. It is mainly used in long-life orifice rings, tank bottom, tank superstructure, perfume-bottle feeder, covers for working tanks and soda lime glass.
 
Applications:
The zircon mullite brick is mainly used in long-life orifice rings, tank bottom, tank superstructure, isostatically pressed, electrode blocks, perfume-bottle feeder, covers for working tanks and soda lime glass, etc.
 
Specifications:
 
| 
			 Item  | 
			
			 ZM-17  | 
			
			 ZM-20 (Zirmul)  | 
			
			 ZM-25 (Vista)  | 
			
			 ZM-30  | 
			
			 ZM-11  | 
		|
| 
			 Chemical composition  | 
			
			 Al2O3  | 
			
			 ≥70  | 
			
			 ≥59  | 
			
			 ≥57  | 
			
			 ≥47  | 
			
			 ≥72  | 
		
| 
			 ZrO2  | 
			
			 ≥17  | 
			
			 ≥19.5  | 
			
			 ≥25.5  | 
			
			 ≥30  | 
			
			 ≥11  | 
		|
| 
			 SiO2  | 
			
			 ≤12  | 
			
			 ≤20  | 
			
			 ≤14.5  | 
			
			 ≤20  | 
			
			 ≤12  | 
		|
| 
			 Fe2O3  | 
			
			 ≤0.5  | 
			
			 ≤0.5  | 
			
			 ≤0.5  | 
			
			 ≤0.3  | 
			
			 ≤0.5  | 
		|
| 
			 Apparent Porosity%  | 
			
			 ≤17  | 
			
			 ≤17  | 
			
			 ≤17  | 
			
			 ≤18  | 
			
			 ≤17  | 
		|
| 
			 Bulk Density g/cm3  | 
			
			 ≥3.15  | 
			
			 ≥2.95  | 
			
			 ≥3.15  | 
			
			 ≥3.10  | 
			
			 ≥3.1  | 
		|
| 
			 Cold Crushing Strength Mpa  | 
			
			 ≥90  | 
			
			 ≥100  | 
			
			 ≥120  | 
			
			 ≥100  | 
			
			 ≥90  | 
		|
| 
			 0.1Mpa Refractoriness Under Load T0.6 ℃  | 
			
			 ≥1650  | 
			
			 ≥1650  | 
			
			 ≥1650  | 
			
			 ≥1650  | 
			
			 ≥1630  | 
		|
| 
			 Permanent Linear Change On Reheating(%)1500℃X2h  | 
			
			 ±0.3  | 
			
			 ±0.3  | 
			
			 ±0.3  | 
			
			 ±0.3  | 
			
			 ±0.3  | 
		|
| 
			 20-1000℃ Thermal Expansion % (x 10-6)  | 
			
			 0-0.6  | 
			
			 0-0.6  | 
			
			 0-0.6  | 
			
			 0-0.6  | 
			
			 0-0.6  | 
		|
| 
			 Thermal Conductivity (Average800℃) W / (M.K)  | 
			
			 ≤ 2.19  | 
			
			 ≤ 2.19  | 
			
			 ≤ 2.1  | 
			
			 ≤ 2.1  | 
			
			 ≤ 2.19  | 
		|
| 
			 Pyrometric Cone Equivalent ℃ SK  | 
			
			 31  | 
			
			 31  | 
			
			 31  | 
			
			 31  | 
			
			 31  | 
		|
 
Competitive Advantage: