Specification of Fused Cast AZS-33
1. Al203 | 49.80% |
2. ZrO2 | 33% |
3. SiO2 | 15.50% |
4. Na20 | 1.40% |
5. Corundum | 47% |
6. Baddeleyite | 32% |
7. Vitreous Phase | 21% |
Bulk Density | 3.7g/cm3 |
Apparent Porosity | ≤1.50% |
Cold Crushing Strength | 350Mpa |
Linear Change Under load | 0 |
RefractorinessUnderLoadof0.2Mpa | 1700℃ |
Exudation Temp | 1400℃ |
Static corrosion of molent glass | 1.45mm/24h |
Blsliter rate | 1.40% |
Features:
AZS-33:It has excellent corrosion resistance to molten glass,a very low exudation and blistering rate .Mainly used in glass contact (side walls ,paving tiles,etc)and superstructures (breast walls ,ports ,tuck-stones,etc)
Typical Applications
Sidewalls
Superstructures
Paving wall
Working ends
Feeder channels
Doghouse arches